Inconel 625 vs Incoloy 825: Which Alloy for Chloride and Acid Service?

Inconel 625 (UNS N06625, W.Nr 2.4856) and Incoloy 825 (UNS N08825, W.Nr 2.4858) are both nickel-based alloys bought for corrosion resistance, and buyers often ask which one to specify. The short answer: Incoloy 825 is the economical choice for sulphuric and phosphoric acid and general chloride stress-corrosion resistance; Inconel 625 is the choice when pitting and crevice corrosion in chlorides, seawater or hot mixed acids is the risk, or when higher strength is needed.

Chemistry at a glance

Element | Inconel 625 (N06625) | Incoloy 825 (N08825)

Nickel | 58.0 min | 38.0–46.0

Chromium | 20.0–23.0 | 19.5–23.5

Molybdenum | 8.0–10.0 | 2.5–3.5

Niobium + Tantalum | 3.15–4.15 | —

Copper | — | 1.5–3.0

Titanium | 0.40 max | 0.6–1.2

Iron | 5.0 max | Balance (about 22 min)

The key difference is molybdenum. 625 carries roughly three times the molybdenum of 825, plus niobium, which is why it resists localised (pitting and crevice) corrosion in chlorides far better. 825's copper addition is what makes it good in sulphuric acid.

Pitting resistance (PREN)

Using PREN = %Cr + 3.3 × %Mo, Inconel 625 comes out at about 50 and Incoloy 825 at about 30–32. In practice, 825 is generally not chosen for stagnant or warm seawater, while 625 is widely used in seawater and chloride-bearing process streams.

Strength

Annealed minimums: Inconel 625 plate to ASTM B443 Grade 1 — tensile 827 MPa, yield 414 MPa. Incoloy 825 plate to ASTM B424 — tensile 586 MPa, yield 241 MPa. The higher strength of 625 often allows thinner walls, which narrows the price gap on a finished-part basis.

Which acid, which alloy?

Sulphuric acid: Incoloy 825 is the classic choice and usually the more economical one.

Phosphoric acid (including wet-process acid with chlorides and fluorides): 825 is widely used; 625 where chloride levels or temperatures are higher.

Hydrochloric acid: neither is ideal at higher concentrations or temperatures; consider Hastelloy B3 or C276.

Chlorides, brines and seawater: Inconel 625.

Mixed oxidising/reducing acids with chlorides: Inconel 625, or Hastelloy C276 / C22 for the most severe service.

Specifications by form

Form | Inconel 625 | Incoloy 825

Plate, sheet, strip | ASTM B443 / ASME SB443 | ASTM B424 / ASME SB424

Round bar | ASTM B446 / ASME SB446 | ASTM B425 / ASME SB425

Seamless pipe & tube | ASTM B444 / ASME SB444 | ASTM B423 / ASME SB423

Welded pipe | ASTM B705 | ASTM B705

FAQ

Q: Is Incoloy 825 cheaper than Inconel 625?

A: Generally yes, because it contains less nickel and molybdenum. Prices track nickel and molybdenum markets, so ask for a current quote on your size.

Q: Can 625 replace 825?

A: In most corrosive services 625 is an upgrade, but check design codes, welding procedure and cost first.

Q: What certificate comes with the material?

A: Every piece from Ganesh Metals ships with the mill's EN 10204 3.1 certificate and heat-number traceability.

Q: Do you stock both?

A: Yes. Ganesh Metals, a stockist, supplier and processor in Mumbai since 1992, supplies Inconel 625 and Incoloy 825 sheet, plate, bar and pipe, with supply across India including SEZ units. Sizes are confirmed per enquiry.

Enquire: call +91 99872 73700 or email sales@ganeshmetals.com with grade, form, size and quantity. See also: Inconel 625 · Incoloy 825 · Hastelloy C276 · metal weight calculator.

GET IN TOUCH
Mahendra Prajapati
📍 Shop Number 12, Sant Sena Maharaj Marg,
2nd Kumbharwada, Mumbai – 400004
📞 +91 99872 73700
📧 sales@ganeshmetals.com
📧 ganeshmetal2372@gmail.com

© 2026 Ganesh Metals. All Rights Reserved.